60% cotton 40% polyester yarn quality issue

  60% cotton & 40% polyester Yarn Quality issue  : 

Yarn quality is considered only for white color sueded order and color is rejected due to very poor pilling-2 and poly contamination in per kg 3.47.


Yarn quality is rejected for white and color due to very poor pilling-1-2 

Yarn quality is ok for white and colored cotton part dyeing for the wash program.


Yarn quality is ok for white and color is considered ok only for sueded orders.


Yarn quality is considered ok for white and color cotton part dyeing seeded and non-sueded orders.


Yarn quality is ok for white color and the color is considered ok two part dyeing only for sueded orders.


Yarn quality is considered ok for white and color (two-part dyeing).


Yarn quality is considered ok for white and Tierra red color two-part dyeing use only for old navy orders.


Yarn quality is considered ok for Tierra red color two-part dyeing approved by the head of the operation sir use only for old navy orders (Pilling Grade-2.5).


we have found excessive neps & dead fiber but commercially ok only for old navy buyers considering only the peach finish.


Yarn quality is considered ok only for color two part dyeing (Except navy, khaki, brown, and olive color) and white color is rejected due to very poor pilling-2.


we have found excessive neps & dead fiber but commercially ok only for old navy buyers considering only the peach finish.


Yarn quality is rejected for white and color two-part dyeing due to major yarn contamination in per kg 8.14 pcs and dead cotton but color is considered ok only for peach finish order (Use only for wash program) After re-check yarn quality is rejected for charcoal marle and midnight marle color cotton part dyeing due to very poor pilling 2-3.


Yarn quality is considered ok for white color and the color is rejected two part dyeing due to major dead cotton but the color is considered ok only for peach finish order (Use only for wash program ).


Yarn quality is considered ok for color two-part dyeing (Pilling-3.5) and Cotton part dyeing is not ok due to very poor pilling-2.5 but commercially ok only for old navy buyer sueded order and white color is rejected due to major yarn contamination per kg 8.48 pcs.


Yarn quality is considered ok for color two-part dyeing (Pilling-4) and white color is rejected due to major yarn contamination per kg 5.21 pcs.


Yarn quality is considered ok for white and color two part dyeing (Excepted navy, khaki, olive, and brown color) But commercially ok only for peach finish order navy, khaki, olive, and brown color (Pilling Grade-4).


Yarn quality is considered ok for the color ctn part and two-part dyeing (Pilling-ctn part-3 and two part-4) and white color is rejected due to major yarn contamination in per kg 8.16 pcs (Pilling white-3.5).


Yarn quality is considered ok for white and peacock green color two-part dyeing only for sueded orders.


Yarn quality is considered ok for peacock green color two-part dyeing only for sueded orders After re-check Yarn quality is considered ok for white use only for sueded orders due to poor pilling-2.


After rechecking Yarn quality is considered ok for the charcoal grey color cotton part and two-part dyeing use only for Walmart Myntra, Walmart Canada, and Meijer buyers, and White color is rejected due to major yarn contamination per kg 5.90 pcs, and another buyer is not ok due to very poor pilling-2.3.


Yarn quality is rejected for white & colored cotton part dyeing due to major thick & thin, very poor pilling-2 and After checking two part dyeing is rejected for lost at sea navy color due to poor pilling-2.


Yarn quality is rejected for color cotton part dyeing due to major neps and pilling, not ok-1-2 but the color is considered ok only for sueded order and white is rejected due to major yarn contamination in per kg 3.75 pcs, neps and pilling, not ok-2 After re-check Yarn test result is consider ok for color two part dyeing (Pilling Grade-3-4).


The yarn test result is rejected for white due to major yarn contamination available and poor pilling-2 and the color cotton part dyeing is rejected due to poor pilling-2.5 After re-check Yarn test result is considered ok for color two part dyeing (Pilling Grade-3-4).


After rechecking Yarn quality is considered ok only for color cotton part dyeing (Pilling Grade-3) and two-part dyeing pilling-2.5 As discussed consider ok for white sueded & aop order and yarn contamination available (Pilling Grade-2).


After rechecking Yarn quality is considered ok for white use only for the old navy (Pilling Grade-2.5) and Color is considered ok the cotton part and two-part dyeing use only for the old navy (Pilling Grade-3).


Yarn quality is considered ok for the color cotton part and two-part dyeing and white is rejected due to major yarn contamination in per kg 8.82 pcs.


The yarn test result is rejected for white due to major neps, yarn contamination per kg 10.37 pcs and pilling, not ok-1-2, and Color has rejected cotton part and two-part dyeing due to major neps, dead cotton, and poor pilling-2 but considered ok only for peach finished order.


The yarn test result is rejected for white due to major yarn contamination in per kg 7.84 pcs and pilling, not ok-1-2, and Color is rejected ctn part dyeing due to poor pilling-1-2 and two-part dyeing color is rejected due to major neps & dead cotton and poor pilling-2 As discuss with consider ok both part dyeing only for peach finished order.


The yarn test result is rejected for white due to major yarn contamination in per kg 3.70 pcs and pilling, not ok-1-2, and Color is rejected ctn part dyeing due to poor pilling-1-2 and two-part dyeing color is rejected due to major neps & dead cotton and poor pilling-1-2 As discuss with consider ok both part dyeing only for peach finished order.


The yarn test result is rejected for white due to major yarn contamination in per kg 9.81 pcs and poor pilling-1-2  and Color is rejected ctn part dyeing due to poor pilling-1-2 and two-part dyeing color is rejected due to major neps & dead cotton and poor pilling-2 As discuss with consider ok both part dyeing only for peach finished order.


The yarn test result is rejected for white due to major neps, yarn contamination per kg 4.22 pcs (Pilling Grade-3) and Color is rejected cotton part and two-part dyeing due to major neps, dead cotton, and poor pilling-2 But both part dyeing color is considered ok only for peach finished order.


The yarn test result is considered ok for white (Pilling Grade-3) and color is considered ok ctn part and two part dyeing is used only for aop and sueded order due to major hairiness and dead cotton (Ctn part pilling-2 and two-part pilling-3).


The yarn test result is considered ok for white use only for sueded order due to major neps and poor pilling-2.5 and the color is considered ok ctn part and two-part dyeing use only for sueded order due to major hairiness and dead cotton (Ctn part pilling-2 and two-part pilling-3).


The yarn test result is considered ok for white (pilling Grade-3) and the color is considered ok two part dyeing (Pilling Grade-3.5) and Cotton part dyeing color is rejected due to major hairiness and poor pilling-1-2.


The yarn test result is considered ok for color ctn part dyeing use only for sueded orders due to major neps and poor pilling-2 two part dyeing color is rejected due to excessive dead cotton and poor pilling-2 and white is rejected due to major yarn contamination in per kg 7.40 pcs and poor pilling-2.


The yarn test result is considered ok for color ctn part dyeing use only for sueded order due to major neps and poor pilling-2 two part dyeing color is rejected due to excessive dead cotton and poor pilling-2 and white is rejected due to major neps, yarn contamination in per kg 5.59 Pcs and poor pilling-2.